All Blogs

Does a Hot Car Deck Raise EV Fire Risk?

By Vignesh Durai · · 5 min read

Not on its own. A hold under a sun-baked deck can peak 20 °C above shade air, still short of runaway onset, but it narrows the margin for a faulty pack.

Not on its own. Measured hold temperatures on tropical voyages peak in the 40s °C, and the upper levels under a sun-heated weather deck can run up to 20 °C above the outside shade. That is hot for a car but well short of the 80–120 °C where a healthy lithium-ion cell starts heating itself. Heat matters by eroding the margin of a pack that is already faulty.

The question matters because car-carrier trades run through some of the hottest sea areas on the planet. Asian exports go to the Gulf, Africa and Latin America, and a ship can sit in a Red Sea or Gulf port on a summer afternoon with its ventilation drawing in air that is itself above 40 °C. The answer shapes where higher-risk vehicles are stowed, what state of charge they travel at, and how detection is set on the upper decks.

45.5 °C
Daytime peak in a ship's upper hold at Guayaquil, Fire Research Note 633
60–70 °C
Steel deck temperatures recorded in the tropics, same study
60 °C / 24 h
Tesla's limit for leaving an EV in ambient heat
80–120 °C
Typical onset of SEI decomposition, the first self-heating step

How hot does a ship's hold actually get?

Hottest just under the weather deck, and close to the outside air lower down. The most detailed published measurements are old but direct. The UK Fire Research Station's Note 633 (1966) analysed continuous hold records from voyages to West Africa and through the Caribbean and Panama to South America. Just below a sun-exposed steel weather deck, the hold averaged 33 °C over eleven days while the outside air sat around 28 °C. In port at Guayaquil, daytime peaks reached 41.0 °C and 45.5 °C.

The steel deck itself reached around 60 °C, and the note cites 70 °C on another voyage. Lower down the hold, temperatures tracked the outside air, and inside the cargo mass the daily cycle disappeared. The authors estimated that a hold's mean could exceed outside shade by up to 10 °C over several days, with daytime peaks about 20 °C higher. They also warned that Red Sea and Gulf ports, with hot land winds and reduced ventilation, could be worse than anything measured.

Is that hot enough to start a battery fire?

No, not for a healthy battery. Lithium-ion cells shipped as dangerous goods must pass the UN 38.3 thermal test, which cycles them between 72 °C and −40 °C, holding at least six hours at each extreme, ten times, without leaking, venting or rupturing. Carmakers set a similar envelope for parked vehicles. Tesla's manuals tell owners to avoid ambient temperatures above 60 °C for more than 24 hours at a time.

The chemistry gives more headroom still. Thermal runaway begins when the solid electrolyte interphase (SEI) on the anode starts to break down, an exothermic step usually placed at 80–120 °C. Some studies report onset as low as the high 50s °C in particular cells. A hold peaking at 45 °C leaves tens of degrees between the ambient and that first reaction.

Heat does not start EV fires on a car deck, but it does start the clock from a higher number. A cell with a latent internal fault self-heats from wherever it begins, and on a hot deck it begins closer to the point of no return.

Where does deck heat actually matter?

With the vehicles that are already compromised. A pack with an internal short, flood corrosion or crush damage generates its own heat. Its temperature is the deck ambient plus that self-heating, so a 45 °C upper deck takes 20–25 °C off the distance to runaway compared with a temperate crossing. The vehicle cannot help itself either. A stowed EV sits in parking or transport mode with its battery cooling off and its battery management system de-energised, so nothing inside the car is drawing that heat away.

Duration adds a second effect. Weeks at high temperature and high state of charge accelerate the side reactions that age a cell, and Tesla's manuals note that an unplugged pack self-discharges at about 1% a day. That is not an ignition source in itself, but it is a reason long hot voyages and high states of charge should not be combined for vehicles of doubtful condition.

What does heat do to fire detection on the upper decks?

It squeezes the margin that absolute thresholds rely on. Marine heat detectors are certified to operate between 54 °C and 78 °C. On an upper car deck already at 45–50 °C in port, a fixed-temperature detector is either close to nuisance alarms or a long way from responding to a small, early heat source. Ventilation cannot cool the space below the outside air. SOLAS requires 6 air changes an hour on cargo ships and 10 on passenger ships while vehicles are aboard, but on a Gulf afternoon every change brings in more hot air.

Detection that watches each vehicle relative to its surroundings handles this better than a deckhead threshold, because a hot deck raises the background for every car at once, while a failing pack rises against its neighbours. That is also why thermal baselines have to be set per deck and per voyage leg rather than once at commissioning.

What should operators on hot routes do?

  • Stow used, repaired, flood-exposed or recalled vehicles on the lower decks, below the waterline where possible, and away from the deck directly under the weather deck.
  • Hold state of charge low for long tropical voyages, especially for vehicles of uncertain history; heat and high charge compound each other.
  • Ventilate when the outside air is cooler than the deck, typically at night and at sea, rather than at a fixed rate through the hottest port hours.
  • Log deck temperatures by level on hot legs, so the crew and the shore team know what 'normal' looks like before something departs from it.
  • Check that detection thresholds on the upper decks were set for tropical conditions, not for a temperate commissioning trial.
Conclusion

How RoRoSAFE helps

On a hot route the upper deck is already warm before anything goes wrong, which is exactly when a single deckhead reading says least. RoRoSAFE watches each parked vehicle's own temperature and battery-vent gases from beneath it, so a developing fault is read at the vehicle rather than through deck air a tropical voyage has already heated. Tiered bridge and shore alerts name the deck and bay. It complements SOLAS detection and suppression; it replaces neither.

Pilot: one deck · installed alongside the berth · no drydock · 6 months of dashboard access

Sources

  • 1. P. C. Bowes — 'High Mean Temperatures in Ships' Holds', Fire Research Note No. 633, Joint Fire Research Organization (UK), October 1966 (BRE Trust archive), read in full: T.S. Dusseldorf (Hamburg–Valparaíso via Panama, 1958) hold mean 33 °C vs outside 28 ± 2 °C over 11 days, 20 in below a sun-exposed weather deck; daytime maxima 41.0 and 45.5 °C at Guayaquil; deck temperatures around 60 °C, 70 °C quoted for another voyage; recommended estimate of up to 10 °C mean excess and about 20 °C peak excess over outside shade; Red Sea and Persian Gulf ports flagged as potentially worse.
  • 2. United Nations — Manual of Tests and Criteria, Section 38.3, test T.2 (thermal test): 72 ± 2 °C and −40 ± 2 °C, at least 6 h at each extreme, 10 cycles, no leakage, venting, disassembly, rupture or fire.
  • 3. Tesla — Owner's manuals (Model 3, Model Y, Model X, Cybertruck), 'High Voltage Battery Information': avoid exposing the vehicle to ambient temperatures above 60 °C or below −30 °C for more than 24 hours at a time; battery self-discharge of about 1% per day.
  • 4. Peer-reviewed reviews of lithium-ion thermal runaway: SEI decomposition as the first exothermic step, typically 80–120 °C, with lower onset reported for some chemistries and states of charge.
  • 5. UN GTR No. 20 and NHTSA FMVSS No. 305a proposal (15 April 2024), as summarised in RoRoSAFE's 'Does Transport Mode Blind an EV's Own BMS?': in usual parking mode the battery cooling is not operating and the BMS is not energised.
  • 6. Lloyd's Register Class News 07/2026 and EN 54 / IEC 60092-504, as summarised in RoRoSAFE's 'Marine-Spec Thermal Cameras on Deck': heat detectors certified to operate between 54 °C and 78 °C.
  • 7. IMO — SOLAS II-2 ventilation requirement for ro-ro spaces: 6 air changes per hour (cargo ships) and 10 (passenger ships) while vehicles are aboard, per IMO SSE 1 summary and MSC.392(95).
Frequently asked

Questions, answered

How hot does a ship's cargo hold get in the tropics?+

Measurements summarised by the UK Fire Research Station found upper holds, just under a sun-exposed weather deck, averaging about 5 °C above outside air, with daytime peaks of 41–45.5 °C in a tropical port. The steel deck itself reached 60–70 °C. Lower in the hold, temperatures stayed close to the outside air.

Can heat alone set an electric car on fire on a ship?+

Not a healthy one. Lithium-ion cells for transport must survive repeated cycling to 72 °C under the UN 38.3 thermal test, and runaway typically starts with SEI decomposition at 80–120 °C. Hold temperatures in the 40s °C are well below that. Heat matters for packs that are already damaged or defective, because it raises the starting point of their self-heating.

What temperature should an EV not be left in?+

Tesla's owner's manuals advise avoiding ambient temperatures above 60 °C or below −30 °C for more than 24 hours at a time. Hold air on hot voyages rarely sustains 60 °C, but the steel weather deck can reach 60–70 °C. Vehicles on the uppermost enclosed deck, directly under that steel, are the ones closest to the limit.

Do hot decks affect fire detection on car carriers?+

They can. Marine heat detectors operate between 54 °C and 78 °C, so an upper deck at 45–50 °C leaves a narrow margin, raising nuisance-alarm risk or delaying response to a small early source. Ventilation cannot cool below the outside air. Detection that compares each vehicle with its surroundings copes better than a fixed deckhead threshold.

Related reading

Continue the thread

BatteryDetection
Oct 4, 2026 · 5 min read

Does Transport Mode Blind an EV's Own BMS?

Largely, yes. A parked EV's BMS can be de-energised with its cooling off, and NHTSA says most single-cell fires start in exactly that state.

By Vignesh DuraiRead
AlgorithmsDetection
Jun 15, 2026 · 2 min read

Setting Anomaly Thresholds: ΔT and Dwell

A trip condition has three axes — magnitude, persistence, and spatial coherence. Get the first two wrong and the third can't save you.

By Vignesh DuraiRead
SensingChemistry
Sep 25, 2026 · 2 min read

The Four Stages of Li-Ion Thermal Runaway

Li-ion runaway moves from SEI breakdown near 80–120 °C through venting to fire. Useful detection works in the venting window, before smoke and flame.

By Vignesh DuraiRead
EVOperations
Sep 9, 2026 · 4 min read

The Argument Over State-of-Charge at Loading

EMSA recommends 20–50% on a PCTC and lines have made 50% a booking condition. What still does not exist is an international requirement.

By Vignesh DuraiRead
EVSafety
Jul 14, 2026 · 3 min read

Are Flood-Damaged EVs a Shipping Fire Risk?

Yes — salt water leaves conductive bridges inside an EV pack that trigger runaway days later. The US Coast Guard tells shippers not to load them.

By Vignesh DuraiRead
CasualtyCargo
Sep 6, 2026 · 5 min read

MSC Flaminia: Ten Days in the Sun

DVB80 booked for a warm-month sailing, then left standing in the sun. Three crew died — and the owner, operator and carrier bore no liability.

By Vignesh DuraiRead
SensingVideo
Aug 30, 2026 · Updated Oct 24, 2026 · 5 min read

Marine-Spec Thermal Cameras on Deck

The spec that decides fitment is not resolution. It is which EN 54 part the camera certifies to, because that fixes which FSS Code duty it can meet.

By Vignesh DuraiRead