All Blogs

Does a Cold Car Deck Lower EV Fire Risk?

By Vignesh Durai · · 5 min read

Slightly, for healthy packs. Cold slows the chemistry, but packs charged hard in the cold can carry plated lithium that self-heats from about 35 °C.

Slightly, for a healthy pack, and not for the packs that matter most. Cold slows the reactions that drive thermal runaway, so a sound battery at −15 °C starts further from trouble than one at 20 °C. Cold in a battery's past is another matter. Cells repeatedly charged in the cold can carry plated lithium. In a 2025 study, cells aged that way began self-heating at about 35 °C instead of about 80 °C. Cold also blunts some of the detectors meant to catch a fire.

This is the winter counterpart to the question of hot decks on tropical routes. It matters most on Nordic and Baltic routes, where the cargo is increasingly electric. Battery-electric cars made up 95.9% of new car registrations in Norway in 2025, according to the Norwegian Road Federation (OFV). For a winter ferry on the Norwegian coast, most of the cars on the deck are now EVs.

How cold does a car deck get?

On a winter route, close to the outside air, because a vehicle deck is ventilated with outside air. SOLAS regulation II-2/20 requires at least 6 air changes an hour on cargo ships and 10 on passenger ships while vehicles are in a closed vehicle space, so the deck air tracks the weather. Open and partly open decks have no buffer at all. Cars also come aboard at the temperature of the quay, so a car that has stood for hours in a sub-zero marshalling lane boards cold-soaked. Battery makers design for this range. Lithium-ion cells shipped as dangerous goods pass the UN 38.3 thermal test, which cycles them between 72 °C and −40 °C. Tesla's manuals advise against leaving a vehicle below −30 °C for more than 24 hours at a time.

95.9%
Battery-electric share of new cars registered in Norway in 2025 (OFV)
~35 °C vs ~80 °C
Self-heating onset of cells aged by cycling at 0 °C vs new cells (Gerosa et al., 2025)
−30 °C / 24 h
Tesla's limit for leaving an EV in cold ambient air

Does cold make a healthy pack safer?

Yes, at the margin. Thermal runaway is a chain of heat-releasing reactions whose rates rise steeply with temperature. A new cell in the 2025 test series did not start self-heating until about 80 °C. A pack sitting at −15 °C on a winter deck is therefore about 95 K short of that point, against about 60 K on a temperate crossing. A latent fault has more ground to make up before it becomes self-sustaining. That is real margin, but it is not protection. An internal short circuit makes its own heat locally, whatever the air around the pack. Once a cell is in runaway, the surrounding temperature does little to slow it.

Where does cold in a battery's history add risk?

In lithium plating. Charging a lithium-ion cell when it is cold slows lithium's movement into the graphite anode, so some of it deposits as metal on the anode surface instead. The clearest recent data come from Gerosa et al. at ZSW Ulm, in the Journal of The Electrochemical Society (2025). They tested commercial 18650 graphite/NCA cells aged by cycling at 0 °C, where plating was the main ageing mechanism. In accelerating-rate calorimetry, the plated cells began self-heating at about 35 °C, against about 80 °C for new cells. They self-heated faster, reached runaway sooner and peaked at about 650 °C, roughly 100 °C hotter than new cells. The temperature at which runaway itself took off was similar, about 203 °C. The plated cells also scored higher EUCAR hazard levels across the abuse tests.

The authors attribute the runaway in plated cells to lithium metal reacting with the electrolyte, not to dendrites piercing the separator. Two limits apply when reading this onto a car deck. These were small cylindrical lab cells, deliberately cycled in the cold, not packs from used cars. And modern battery management systems cut charging current at low temperature and preheat the pack before fast charging, precisely to avoid plating. The exposure sits with packs whose thermal management failed, was bypassed or was never fitted. Those are the vehicles that also turn up in used-EV export flows from cold markets.

A cold deck lowers the starting temperature of every pack. A cold-charging history can lower the temperature at which a damaged cell starts to heat itself. The first is a property of the voyage. The second travels with the car, and the loading paperwork rarely records it.

What does cold do to fire detection on the deck?

It widens the gap that fixed thresholds have to cross, and it slows some sensors. Marine heat detectors are certified to alarm between 54 °C and 78 °C. From a 20 °C deck, a fixed-temperature head needs a rise of at least 34 K. From a −10 °C deck it needs at least 64 K, so a small early heat source stays invisible for longer. Electrochemical gas sensors lose sensitivity and respond more slowly as they cool. Analog Devices notes the loss becomes significant below about −30 °C. Cold-loaded cars also warm towards the deck temperature for hours after boarding, which shifts the thermal background of the whole deck at once. A failing pack shows up against that background as a vehicle warming faster than its neighbours, not as a reading above a fixed line.

Condensation is the cold-route problem that sounds worse than it is. When warm, moist air meets a cold-soaked car, water condenses on it: the cargo sweat that P&I clubs warn about for steel and grain. On vehicles, that is a corrosion and claims issue for exposed electrics and connectors. We found no published case of it igniting a sealed traction pack.

What should operators on winter routes do?

  • Don't count the cold as a safety margin for vehicles of doubtful history. Used, repaired or flood-exposed EVs from cold markets are where plating risk concentrates.
  • Ask about charging history and thermal-management faults for used EVs, alongside state of charge, where the shipper can supply it.
  • Check that heat and gas detectors on open and partly open decks are rated for the lowest temperatures on the route, and include winter conditions in detector testing.
  • Set thermal baselines that track the deck as cold-loaded cars warm up, so a pack heating faster than its neighbours stands out from the general rise.
Conclusion

How RoRoSAFE helps

On a winter route every car comes aboard cold and warms for hours, so a fixed deckhead threshold says least just when a pack with a cold-charging history may be heating itself. RoRoSAFE reads each parked vehicle's own temperature and battery-vent gases from beneath it, so a pack warming faster than its neighbours stands out against the deck. Tiered alerts reach the bridge and shore naming the deck and bay, alongside the ship's SOLAS detection.

Pilot: one deck · installed alongside the berth · no drydock · 6 months of dashboard access

Sources

  • 1. Gerosa, G.G., Feinauer, M., Hogrefe, C., Häfele, S., Bischof, K., Wörz, M., Böse, O., Wohlfahrt-Mehrens, M., Hölzle, M. and Waldmann, T. (ZSW Ulm / HIU), 'Impact of Testing Method on Safety Assessment of Aged Li-ion Cells: Part I — Li Plating as Main Aging Mechanism', Journal of The Electrochemical Society 172 (2025) 030502, DOI 10.1149/1945-7111/adb804, open access, read in full: commercial 18650 graphite||NCA cells aged by cycling at 0 °C; ARC self-heating onset about 35 °C (plated) vs about 80 °C (new); thermal-runaway temperature about 203 °C for all cells; venting 121–133 °C; Tmax about 650 °C for plated cells, almost 100 °C above new cells; shorter time to runaway; higher EUCAR hazard levels; runaway in plated cells attributed to lithium metal reacting with electrolyte, not dendrite shorts.
  • 2. Norwegian Road Federation (OFV) — 2025 new passenger car registrations: battery-electric share 95.9% (172,233 of 179,549), up from 88.9% in 2024.
  • 3. IMO — SOLAS regulation II-2/20.3.1, ventilation of closed vehicle and ro-ro spaces: at least 6 air changes per hour on cargo ships and 10 on passenger ships.
  • 4. UN Manual of Tests and Criteria, section 38.3, test T.2 (thermal test): cycling between 72 °C and −40 °C.
  • 5. Tesla — Owner's manuals, 'High Voltage Battery Information': avoid exposing the vehicle to ambient temperatures above 60 °C or below −30 °C for more than 24 hours at a time.
  • 6. IMO — FSS Code chapter 9, paragraph 2.3.1.3: heat detectors to operate between 54 °C and 78 °C when the rate of rise is under 1 °C per minute. The 34 K and 64 K rises are RoRoSAFE's arithmetic from the 54 °C lower bound.
  • 7. Analog Devices — 'Overcoming the Technical Challenges of Electrochemical Gas Sensing': sensitivity and responsiveness decrease significantly below about −30 °C.
  • 8. Steamship Mutual — 'The Problem of Sweat' (April 2025); London P&I Club, LP Focus (February 2016): cargo sweat forms when warm, moist air meets cold cargo.
Frequently asked

Questions, answered

Is an EV less likely to catch fire on a cold car deck?+

A healthy one, slightly. Cold slows the reactions behind thermal runaway, so a pack at −15 °C sits about 95 K below the roughly 80 °C at which a new cell begins self-heating. That margin does not stop an internal short making its own heat, and it does little once a cell is already in runaway. For vehicles with a damaged or cold-charged pack, cold is not a safety margin.

Why does charging a battery in the cold matter for shipping?+

Because cold charging can plate metallic lithium on the anode. In a 2025 study of commercial 18650 cells aged by cycling at 0 °C, plated cells began self-heating at about 35 °C instead of about 80 °C. They also reached runaway sooner and burned about 100 °C hotter. Modern battery management limits cold charging, so the risk concentrates in packs whose thermal management failed or was bypassed.

Do heat detectors work as well on a cold vehicle deck?+

They take longer. Marine heat detectors alarm between 54 °C and 78 °C, so from a −10 °C deck a fixed-temperature head needs a rise of at least 64 K, against 34 K from 20 °C. Electrochemical gas sensors also lose sensitivity and response as they cool, markedly below about −30 °C. Detection that compares each vehicle with its neighbours is less affected by a cold background.

Can condensation on cold cars start a battery fire at sea?+

We found no published case of that. Cold-soaked cars meeting warm, moist air collect condensation, the cargo sweat P&I clubs warn about for other cargoes. On vehicles it is a corrosion and claims issue for exposed electrics and connectors. Traction packs are sealed enclosures, and the documented cold-weather battery hazard is lithium plating from charging, not moisture on the outside.

Related reading

Continue the thread